abstract |
A biodegradable nonwoven web comprising substantially continuous multicomponent filaments is provided. The filaments comprise a first component and a second component. The first component contains at least one high-melting point aliphatic polyester having a melting point of from about 160° C to about 250° C and the second component contains at least one low-melting point aliphatic polyester. The melting point of the low-melting point aliphatic polyester is at least about 30° C less than the melting point of the high-melting point aliphatic polyester. The low-melting point aliphatic polyester has a number average molecular weight of from about 30,000 to about 120,000 Daltons, a glass transition temperature of less than about 25° C, and an apparent viscosity of from about 50 to about 215 Pascal-seconds, as determined at a temperature of 160° C and a shear rate of 1000 sec-1. |