http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007029586-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_56af5c875e5d95f7ac9660e894a32b15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cdd94f212dc7aef02fc1dcf28fa9b4fd |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-844 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 |
filingDate | 2006-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e6efddd347a19a60c409217335bf795 |
publicationDate | 2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2007029586-A1 |
titleOfInvention | Method for manufacturing organic electroluminescent device |
abstract | Disclosed is a method for manufacturing an organic EL device wherein production load during formation of a protective film is decreased without lowering the protective resistance to moisture or oxygen. Specifically disclosed is a method for manufacturing an organic electroluminescent device wherein a protective film is formed over an organic electroluminescent device which is formed on a substrate. In this method, the step for forming the protective film is composed of a step (103) for forming a first protective film in a vacuum environment, and a step (104) for forming a second protective film in an atmospheric pressure environment. |
priorityDate | 2005-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.