Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2be5e6568abf409d1328c58518da8939 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c72d118f5664072de841f9c5c34b9d99 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e05ab37f556ce3d41d120fc94b3d9ec2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0846 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-147 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-10 |
filingDate |
2005-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c6cea13f312fee45e0dab4f29d0933ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_939b02924b33a584552c32b62bd7255f |
publicationDate |
2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2007013890-A2 |
titleOfInvention |
Thermoplastic wear resistant compositions, methods of manufacture thereof and articles containing the same |
abstract |
Disclosed herein is a composition comprising a polycarbonate resin; a polycarbonatepolysiloxane copolymer; and an anhydride modified polyolefin. Disclosed herein too is a composition comprising a blend of a polycarbonate resin with a polycarbonatepolysiloxane copolymer; and an anhydride modified polyethylene, wherein the composition has a wear factor of less than or equal to about 350 in5min/ftlb-hr and an impact strength of greater than or equal to about 500 joules per meter, and wherein the wear factor is measured according to the formula: Wear Factor= [(6.1 x10 8 )(W)]/[(PxV) x (D) x (T)] where P is the applied pressure in pounds per square inch and V is the velocity in feet per minute, W is the weight loss in grams, D is the density in grams per cubic centimeter and T represents 100 hours. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105942872-A |
priorityDate |
2004-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |