http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006138406-A3

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d648658dd620f548c24de39659a5e9e3
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B2009-168
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B2009-165
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-86
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-866
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-89
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-88
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-00
filingDate 2006-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ed27b2f0976ca16ecf63148ad41f896
publicationDate 2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber WO-2006138406-A3
titleOfInvention High intrinsic viscosity melt phase polyester polymers with acceptable acetaldehyde generation rates
abstract A method for the production of solid polyester polymer particles comprising: a) polycondensing a molten polyester polymer composition in the presence of a polycondensation catalyst composition comprising antimony species; b) continuing the polycondensation of the molten polyester polymer composition to an It.V. of 0.68 dL/g or more; and c) after reaching an It.V. of 0.68 dL/g or more, adding a catalyst stabilizer or deactivator to the polymer melt; and d) after reaching an It.V. of 0.68 dl&lowbar;/g or more, solidifying the melt into solid polyester polymer particles which do not contain organic acetaldehyde scavengers. In a further embodiment, after solidification of the polyester from the melt phase polycondensation process: e) the amount of residual acetaldehyde in the particles in the solid state is reduced to a level of 10 ppm or less without increasing the It.V. of the particles by more than 0.03 dl&lowbar;/g. Such particles having an AA (acetaldehyde) generation rate of 20 ppm or less upon being melted after solidification following the melt phase production and a free AA level reduced after melt phase production to 10 ppm or less are introduced into a melt processing zone to make articles such as bottle preforms having acceptable levels of residual AA.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8901272-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8987408-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8557950-B2
priorityDate 2005-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6569479-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6384180-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6489434-B2
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419558760
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID177
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5354495
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419549163

Total number of triples: 31.