http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006050927-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0d1cd9dcd4f6e73fb4457ef449865cdb http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ef7ed033ebbe18e7a7d1a6900da99cfd |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10981 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10247 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-0852 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-8048 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-722 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-1077 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-32 |
filingDate | 2005-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2551895f8b63cb9e0df128d9e8b2475b |
publicationDate | 2006-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2006050927-A1 |
titleOfInvention | Method for producing a laminated glass, and laminated glass itself |
abstract | The invention relates to a method for producing a laminated glass (1), during which at least one support glass (2) is pretreated with an adhesion promoter (4), and at least one layer made of resin (3) is subsequently applied two-dimensionally to the support glass (2). Once this is completed, a laminated glass (1) can be manufactured that has UV resistance, fulfills the requirements of a laminated safety glass and, furthermore, can be produced in a simplified and cost-effective manner. To this end, the resin (3) comprises a liquid, UV-resistant 1K polyurethane material that contains, in essence, one prepolymer based on an aliphatic isocyanate with small monomeric portions, and a temperature of up to approximately 30 °C is provided for curing the resin. In addition, the aim of the invention is to create a laminated glass (1) comprising at least one support glass (2) and at least one layer made of resin (3), which has UV-resistance, fulfills the requirements of a laminated safety glass, and which is produced in a simplified and cost-effective manner. To this end, the resin (3) is a liquid, UV-resistant 1K polyurethane material containing, in essence, one prepolymer based on an aliphatic isocyanate with small monomeric portions. |