Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4dd77fb6c28df871fd8baf18b22ea42e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8705e57e695d7b32cfd1170ff7b6eb28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b4cc8283dd5112c85aeb567da229d0c3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-756 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-0502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-60 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D24-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D99-0089 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-00 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-24 |
filingDate |
2005-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_edb6ffac9a15ebd9a9486c76192ca9e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f651432b0afcc7422059e6a9045bf919 |
publicationDate |
2006-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2006022341-A1 |
titleOfInvention |
Process for production of submicrohoneycomb structures |
abstract |
A process for the production of a honeycomb-like porous body of 10 to 1000nm in thickness which is made of a water-insoluble polymer and has pores having diameters of 10 to 100nm, which comprises the following steps: (1) the step of dissolving a water-insoluble polymer in a water-incompatible organic solvent having a surface tension (ϜL) of 50dyn/cm or below to prepare a solution of the polymer in the organic solvent, (2) the step of applying the solution prepared in the step (1) to the surface of a substrate with the proviso that the surface tension (ϜS) of the substrate, the surface tension (ϜL) of the organic solvent, and the surface tension (ϜSL) between the substrate and the solvent satisfy the relationship: ϜS - ϜSL > ϜL, and (3) the step of bringing the solution applied on the substrate into contact with air having a relative humidity of 30 % or above to evaporate the organic solvent at such a rate that the coating thickness at applying the solution to the surface of the substrate is reduced by a factor of 5 within one second. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010134440-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009073983-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014065229-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011202100-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010037554-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007291185-A |
priorityDate |
2004-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |