Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d648658dd620f548c24de39659a5e9e3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-582 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-6856 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-916 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-1535 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-1535 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 |
filingDate |
2005-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2af93ee42f939ac7a341342c4a248bb3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4ab85b1eb7ff90fed7a324a9dd75291 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_efd1b317fd953cba7486c1a609204ccc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3795928cbbbb91294ad2a32f4f107efd |
publicationDate |
2005-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2005118671-A1 |
titleOfInvention |
Process for adding furyl-2-methylidene uv light absorbers to poly(ethylene terephthalate) |
abstract |
A method for incorporating a UV light absorbing compound into a polyester prepared using direct esterification of reactants selected from a dicarboxylic acid and a diol, the method comprising reacting the reactants in an esterifying reactor under conditions sufficient to form an esterified product including at least one of an ester, an oligomer, or mixture having an ester and a mixture of low molecular weight polyester; polymerizing the esterified product in a polycondensation reactor to form a polyester; and adding the UV absorbing compound to the esterified products when at least 50% of the carboxy groups initially present in the reactants have been esterified to obtain a yield of UV absorbing compound incorporated into the polyester of greater than 40%. Articles utilizing the UV protected polyester are additionally disclosed. |