Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1dd98ad4ee076841fec541542f952f58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_46295cb79aafd275599d9a057b104f19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1291077b0a1913e579b8b76f0cdca062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4787b097429b6b2eb11fa1cc155df46e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b888ed6920726f67662bb1844537b228 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B13-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82B3-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B13-32 |
filingDate |
2005-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c6e093e4dcc30808f6be4677b68d63c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac8b2f34004a75dc9726ca8d2235b0be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46a3061ef8104a7b5aecb4e4474ed6c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e5109f76aabdaee21c527a0c169dee9 |
publicationDate |
2005-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2005113427-A2 |
titleOfInvention |
Process for preparing nano-sized metal oxide particles |
abstract |
The present invention is directed to novel sol-gel methods in which metal oxide precursor and an alcohol-based solution are mixed to form a reaction mixture that is then allowed to react to produce nanosized metal oxide particles. The methods of the present invention are more suitable for preparing nanosized metal oxide than are previously-described sol-gel methods. The present invention can provide for nanosized metal oxide particles more efficiently than the previously-described sol-gel methods by permitting higher concentrations of metal oxide precursor to be employed in the reaction mixture. The foregoing is provided by careful control of the pH conditions during synthesis and by ensuring that the pH is maintained at a value of about 7 or higher. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008137843-A |
priorityDate |
2004-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |