abstract |
A method for producing a green sheet, which comprises a step of providing a green sheet before compression containing a ceramic powder and a binder resin, and a step of compressing the above green sheet before compression, to form a green sheet after compression, characterized in that a sheet compression ratio (Δρg/ρg1) is 1 % or more, wherein the difference (Δρg) between a sheet density before compression (ρg1) of the green sheet before compression and a sheet density after compression (ρg2) of the green sheet after compression is represented as Δρg = ρg2 - ρg1, and the ratio of the difference (Δρg) to the sheet density before compression (ρg1) is represented as the sheet compression ratio (Δρg/ρg1). |