Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0d34055d3d63a1093a8e57bf15d990e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9f8f4cb9e4da9d9870a2d2dbf4c7a0f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dfbfbd26409fa3b6b0ba616257690419 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1d29f7ac2c7f9be9f7dae1a83bbb5c92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af8608f2932f41f5c14ec3fb2563461b |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00844 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N10-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N10-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-56 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L35-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L35-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-52 |
filingDate |
2005-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22aa0fd4ebffb43e9202f5d773b45cb4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25fce4f9d7548f148d7bd3ab97176342 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1687cd0ba0e471b7a0e4f9676c81de93 |
publicationDate |
2005-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2005075382-A1 |
titleOfInvention |
Metallized ceramic molding, process for producing the same and peltier device |
abstract |
[PROBLEMS] To provide a metallized nonoxide ceramic molding that exhibits enhanced bonding strength between metal layer and substrate and enhanced boding durability, and provide a process for producing the same. [MEANS FOR SOLVING PROBLEMS] The process for producing a metallized molding is characterized by including the heating step of heating a nonoxide ceramic molding to a temperature 300°C lower than the oxidation initiation temperature of the nonoxide ceramic or higher temperature substantially without solid dissolution of oxygen during the temperature rise; the oxidation step of bringing the nonoxide ceramic molding, as a substrate, heated by the heating step into contact with an oxidative gas and maintaining the same at a temperature higher than the oxidation initiation temperature of the nonoxide ceramic so that the nonoxide ceramic molding has its surface oxidized to thereby form an oxide layer; and the metallizing step of forming a metal layer on the surface of the oxide layer of the nonoxide ceramic molding having the oxidized layer provided on its surface in the oxidation step. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10224472-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4772507-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005070851-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015030220-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017152715-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017191816-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010531050-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015050273-A |
priorityDate |
2004-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |