Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_adb0e564374fedf34b36103d36e6455a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_26bf32076f97973d2313356c279694df http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_77045cbfef954fe70eecd027732e4495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e89624769740892689d99488f3a51c89 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-18 |
filingDate |
2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5bbf9c4b079011588f6bfb690742f49d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a529e72b5503daaef06d2c8e74477e2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0feedec53417a378087e6d1e32b41944 |
publicationDate |
2003-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-03099927-A1 |
titleOfInvention |
Process for making a thermoplastic composition comprising dynamic cross-linking |
abstract |
The invention relates to a process for making a thermoplastic composition comprising dynamic cross-linking of a composition comprising a thermoplastic matrix polymer A having functional groups reactive with epoxide groups and 25-80 mass% based on polymer A of a polymer B having epoxide groups and secondary hydroxyl groups, and optionally other components. This process omits separate addition of a cross-linking agent, because the polymer B is self-crosslinking above a certain temperature. A further advantage is that the risk of undesired side-reactions, e.g. leading to degradation of polymers in the blend is reduced. Another advantage is that cross-link density of polymer B can be varied up to relatively high cross-link densities, by varying the total amount of functional groups or the ration of epoxide to secondary hydroxyl groups. With this process products with improved properties are obtained. The invention further concerns the product obtainable by said process, and use thereof as the thermoplastic elastomer or impact-modifier. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018100514-A1 |
priorityDate |
2002-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |