http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03012798-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2933 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-294 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2962 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-05 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-301 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-441 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L81-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 |
filingDate | 2002-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_956ab140288245d1d61f792e674607ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8a4ef85b80157a87576c0dc6d2fac08 |
publicationDate | 2003-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-03012798-A1 |
titleOfInvention | Polyphenylene sulfide alloy coated wire |
abstract | The present invention relates an electrically conductive wire having a metal core and an outer electrically insulative, polymer coating wherein the polymer composition contains polyphenylene sulfide, a polymeric grafting agent and an ethylene copolymer. The polymeric grafting agent is a copolymer of at least about 50% by weight ethylene, about 0.5% to about 15% by weight of a reactive comonomer selected from the group consisting of: (i) an unsaturated epoxide of 4-11 carbon atoms, (ii) an unsaturated isocyanate of 2-11 carbon atoms, (iii) an unsaturated alkoxy silane and/or unsaturated alkyl silane wherein the alkoxy or alkyl group is from 1-12 carbon atoms, and (iv) an oxazoline; and about 0 to about 49% by weight of a third optional comonomer selected from at least one of an alkyl acrylate, alkyl methacrylate, vinyl ether, carbon monoxide, and sulfur dioxide, where the alkyl and ether groups are of 1-12 carbon atoms. The ethylene copolymer comprises at least about 50% by weight ethylene, about 1% to about 35% by weight of an acid-containing unsaturated mono-carboxylic acid, and about 0 to about 49% by weight of a moiety selected from at least one of alkyl acrylate, alkyl methacrylate, vinyl ether, carbon monoxide, and sulfur dioxide, and further wherein the acid groups are neutralized from 0-100% by a metal ion. Such wire meets SAE J1678 specifications at 125°C or higher at a thickness of polymeric coating of less than 12 mils and/or withstands temperatures as high as 150°C at a thickness of polymeric coating of from 15 mils to 30 mils. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019106171-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005106898-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111417684-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005106898-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7771819-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009105527-A1 |
priorityDate | 2001-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 158.