Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44574bc9b2482dc9ad2d6b7446dd95dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a12b0be1b74901f556d1d1a9200529ce http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc6b1672f3e6d9609e0e2b4d1a5f8ab2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_30f55461db087ca02b693e187faae48b |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 |
filingDate |
2001-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_80d67bc452c97488e66f2fe3e8216020 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9ff981591cc973be65cf7a9b8ec1314 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec0a8e14fd83e85710ccc7cc721d55f2 |
publicationDate |
2002-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-0250202-A1 |
titleOfInvention |
Method for preventing misting when coating flexible supports with a crosslinkable liquid silicone composition, in a device comprising rollers |
abstract |
The invention concerns a method for preventing misting when coating flexible supports with at least a liquid silicone (RTV polyaddition) composition precursor of silicone coating(s), with a coating device comprising rollers operating at high speed. The invention aims at increasing misting speed and consequently enhancing the appearance, the mechanical properties of the silicone coating, as well as industrial hygiene. Therefor, it consists in using a liquid coating composition obtained by mixing: a silicone phase comprising one or several POS (A) and optionally one or several (crosslinking) compound(s) (B) having a viscosity eta at 25 DEG C ranging between 100 and 800 mPa's; with 1 to 10 wt. % of an anti-misting aqueous silicone (water-in-oil) emulsion having an aqueous phase phi a comprising at least 20 wt. % of water; and optionally with a water/solvent liquid (D). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8685499-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008155374-A1 |
priorityDate |
2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |