http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0228632-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b2d4c4ba207a660bd603903e0509d7cc |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-622 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B33-04 |
filingDate | 2001-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_add47ae5a28de74f9afa7a5008989d27 |
publicationDate | 2002-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-0228632-A1 |
titleOfInvention | Process for making clay spheroids |
abstract | A process of making ceramic spheroids by firing clay spheroids comprising by weight percent: FeO (3.22-5.21), Fe3O4 (3.40-5.11), SiO2 (52.49-59.42), CaO (1.99-7.96), MgO (2.81-4.69), A12O3 (12.05-17.65), T1O2 (0.58-0.71), MnO (0.07-0.19), Na2O (0.47-0.86), K2O (1.70-2.37), P2O3 (0.13-0.19), S (0.03-0.29), CO2 (0.90-8.23), Organic C (0.22-1.04), H2O+ (4.14-7.28), H2O- (2.12-5.48) in contact with a particulate parting agent selected from aluminum oxide, magnesium oxide, and their precursors at a sufficiently high temperature and for a sufficiently long time to form a shell. Preferably, the clay spheroids are obtained from a deposit located at Hallock in Kittson County Minnesota, U.S.A.. |
priorityDate | 2000-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |