Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7dd51746dca5083a3697caa79e9ea562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8b9b07baa39efdd68eb1506a375245f8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31551 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-0819 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F283-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L79-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 |
filingDate |
2000-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ef693dc1354aa5eb79b00666668e8b6 |
publicationDate |
2001-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-0136552-A1 |
titleOfInvention |
Waterborne primer with improved chip resistance |
abstract |
The invention provides a thermosetting aqueous primer composition that includes a dispersed polyurethane polymer, an acrylic polymer emulsion polymerized in the presence of the polyurethane dispersion, and a crosslinking component that is reactive with at least one of the polyurethane polymer and the acrylic polymer. The polyurethane polymer has a glass transition temperature of O °C or less. The acrylic polymer has a glass transition temperature that is at least about 20 °C higher than the glass transition temperature of polyurethane resin. The invention further provides a composite coating having as a primer layer a cured layer of the primer composition of the invention and having at least one topcoat layer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10799912-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3036046-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112236484-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106833212-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106046305-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106833212-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021221993-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003213206-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105473233-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100940452-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019233980-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9962735-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10633546-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03064549-A1 |
priorityDate |
1999-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |