Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e0af72a69db64eacd1235d8e64376ddf http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cf41d08a8be8e71799fcb3fe11dd4562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f01735121b3f50ea5bcede17589b52b2 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-1345 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 |
filingDate |
1999-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6deb0b167330be67d6420b197d0adfc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93724694080109c43b830ab05fe5c0cc |
publicationDate |
2000-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-0008096-A1 |
titleOfInvention |
Stabilizing mixture having a melting point lower than that of the highest melting component |
abstract |
Stabilizing mixture comprising: (a) tetrakis [3-(3,5-di-t-butyl-4-hydroxyphenyl)propionyloxymethyl]methane; (b) octadecyl-3-(3',5'-di-t-butyl-4'-hydroxyphenyl)propionate; characterized in that it has a melting point ranging from 50 °C to 60 °C. The above mixture can be used as stabilizer for the oxidative degradation of organic polymers caused by light and/or heat. |