Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_78ca80ad4b743c901ec136b21263f093 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-02 |
filingDate |
2015-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0efbc44823304c6bca40053791af0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2baaa6bbdd46e30d1f3dac345ddf7e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae84d7e05964cc115acdaaafaa6de242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce32c0ae07cdbb8c77f38aee3b6a8a8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bbe7ed0a724832c838cf716953eab31 |
publicationDate |
2018-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-9897722-B2 |
titleOfInvention |
Optically diffusive plastic having high stiffness |
abstract |
An optically diffusive plastic can comprise 40 to 94.9 mass % of a polymer resin matrix; 5 to 50 mass % of a glass filler; and 0.1 to 10 mass % of a light diffusing component; wherein the difference between refractive index of the polymer resin matrix and refractive index of the glass filler is less than or equal to 0.02; wherein a 1 millimeter (mm) thick sample of the optically diffusive plastic comprises a DLD value of greater than or equal to 1 degree (°) as measured by goniophotometry; wherein the 1 mm thick sample comprises a total transmittance of greater than or equal to 40% for incident light having a wavelength of 360 nanometers (nm) to 750 nm in air; and wherein a 3.2 mm thick sample of the optically diffusive plastic comprises a flexural modulus, measured at 23° C., of greater than or equal to 2,500 Megapascal (MPa). |