abstract |
A composition for a window film includes a siloxane resin represented by Formula 1, 4 or 7, or a mixture thereof, and an initiator. A flexible window film is manufactured using the same, and has a pencil hardness of about 7H or higher, a radius of curvature of about 5.0 mm or less, and a difference in yellow index before and after irradiation (ΔY.I.) of about 5.0 or less. A flexible display includes the flexible window film.n n(R 1 SiO 3/2 ) x (R 2 R 3 SiO 2/2 ) y Formula 1n n(R 1 SiO 3/2 ) x (R 9 SiO 3/2 ) z Formula 4n n(R 1 SiO 3/2 ) x (R 2 R 3 SiO 2/2 ) y (R 9 SiO 3/2 ) z Formula 7 |