Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0036 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0425 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-15 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D9-02 |
filingDate |
2013-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2017-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5fdb97cdc8e62d0facdc01cb3d3fd5cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de331036700da249c2c87e20ec00d205 |
publicationDate |
2017-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-9734953-B2 |
titleOfInvention |
Carbon paste and solid electrolytic capacitor element |
abstract |
A carbon paste including a carbon powder, a resin, and an oxygen releasing oxidizer. The amount of the oxidizer is 3 to 30 parts by mass based on 100 parts by mass of the total amount of the carbon powder and the resin. A solid electrolytic capacitor element is prepared by a method which includes making a valve-action metal powder sintered to obtain an anode body, electrolytically oxidizing a surface of the anode body to chemically convert the surface into a dielectric layer, electrolytic polymerization to form a semiconductor layer of an electro conductive polymer on the dielectric layer, applying the carbon paste onto the semiconductor layer, and drying and hardening the carbon paste to form a carbon layer. |