abstract |
Provided are a thinner composition for improving coating property of a resist and for removing the same, which includes 10 to 80 wt. % of alkyl (with 1 to 5 carbon atoms) 2-hydroxyisobutyrate, 20 to 90 wt. % of propyleneglycol alkyl (with 1 to 5 carbon atoms)ether acetate, and 10 to 1000 ppm of a surfactant represented by Formula 1 to a total weight of the alkyl 2-hydroxyisobutyrate and propyleneglycol alkylether acetate, so as to achieve excellent solubility to various photoresists and bottom anti-reflective coatings (BARC) and high edge bead removing (EBR) performance, possibly be employed in a process for recycling photoresist-coated wafers, and remarkably improve coating property of the photoresist, and a method for manufacturing a semiconductor device or a thin film transistor liquid crystal display device including removal of the photoresist by using the above-described thinner composition. |