Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_faf522b8b83eded745c73018576219ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_42877653950ae652e0e77ad480a12a72 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P30-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P30-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3085 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J29-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 |
filingDate |
2013-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2016-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0459f13fbb29b9c6e09342374f16ebb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d564e78327bfa02680726a2a3cf93768 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ae8590879d92606200458a1aa48e799 |
publicationDate |
2016-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-9468916-B2 |
titleOfInvention |
Method for producing PAU zeolite |
abstract |
Provided is a method that is for producing a PAU zeolite and that can have an environmental impact that is reduced while, as much as possible, not using a structure-defining agent. The method for producing a PAU zeolite produces by means of (1) mixing a silica source, an alumina source, an alkali source, and water in a manner so as to result in a reaction mixture having a composition represented by a specific mole ratio, (2) using as the seed crystal a PAU zeolite that does not contain organic compounds and has a SiO 2 /Al 2 O 3 ratio of 4-15 and an average particle size of at least 100 nm, and adding same to the reaction mixture at a ratio of 0.1-20 wt % with respect to the silica component in the reaction mixture, and (3) subjecting the reaction mixture to which the seed crystal has been added to sealed-vessel heating at 80-200° C. |