abstract |
In order to provide a rubber composition having high transparency and toughness, the present invention can provide a crosslinked rubber composition, being substantially free of silica, comprising a first olefin polymer having refractive index of between 1.500 to 1.525 at 23 degree C.; and a second olefin polymer which is different from the first olefin polymer, wherein the composition has haze of 20% or less on 2 mm thick sheet, measured according to JIS K7136, and wherein the composition has Type A Durometer hardness (0 sec) of 35 or more, measured according to JIS K6253. |