http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9376574-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_41ac7ff6ab574ca3737b892da2ebfe6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ac17835c97e6c72213815ca74845386 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ce297fff9638f95d90649f1c8fcaa335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_81500c118cbe2d19979ddb6188070138 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_55718e207cc119c833271f2ad57b5809 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-037 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F257-02 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F257-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-03 |
filingDate | 2009-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05fc5ffbaaa0966ce5801c6820eb908a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b03cc4b13643abf9a3b61b657c331832 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adc474788a75c9afce10279bfb6b32d4 |
publicationDate | 2016-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-9376574-B2 |
titleOfInvention | Method for forming multilayer coating films wherein the basecoat film comprises acrylic, polyester and melamine resins, carbodiimide and urethane thickeners |
abstract | The present invention relates to a method for producing a multilayer coating film, which comprises steps of applying a waterborne intermediate coating composition on an electrodeposited coating film to form an intermediate coating film; applying a waterborne base coating composition on the intermediate coating film to form a base coating film; applying a clear coating composition on the base coating film to form a clear coating film; and simultaneously baking and curing the intermediate coating film, the base coating film applied thereon, and the clear coating film further applied thereon in order to form a multilayer coating film, wherein the waterborne intermediate coating composition comprises an emulsion of a hydroxyl group-containing acrylic resin comprising 27 to 65% by weight of a styrene monomer, wherein the emulsion has a water-tolerance within a range of from 0.2 to 5 and a hexane-tolerance within a range of from 5 to 25; a hydroxyl group-containing polyester resin; a melamine resin; a carbodiimide; and an associative thickener, wherein the associative thickener comprises an urethane compound (A) represented by the formula (1), and an urethane compound (B) represented by the formula (2): R—(OA) m -O—C(═O)—NH—Y—NH—C(═O)—O-(AO) n —R (1) R—(OA) a -[O—C(═O)—NH—Y—NH—C(═O)—(OA) b ] c -O—C(═O)—NH—Y—NH—C(═O)—O-(AO) d —R (2) wherein R independently represents a hydrocarbon group having 8 to 24 carbon atoms, Y independently represents a residue resulted from a removal of two isocyanate groups from a diisocyanate, OA independently represents an oxyalkylene group having 2 to 4 carbon atoms, AO independently represents an alkyleneoxy group having 2 to 4 carbon atoms, O represents an oxygen atom, C represents a carbon atom, N represents a nitrogen atom, m independently represents an integer of 20 to 500, n independently represents an integer of 20 to 500, a independently represents an integer of 1 to 100, d independently represents an integer of 1 to 100, b represents an integer of 40 to 500, c represents an integer of 1 to 5, b by c (or b×c) represents an integer of 150 to 2500, and R may be the same or different, and Y may be the same or different, wherein each of the urethane compounds (A) and (B) has at least 80% by weight of oxyethylene groups and ethyleneoxy groups relative to the total weight of the oxyalkylene groups and the alkyleneoxy groups, wherein weight ratio of the hydroxyl group-containing acrylic resin emulsion to the associative thickener is within a range of from 100/0.1 to 100/50 as a basis of the solid content, in order to provide the multilayer coating film with an excellent exterior appearance by a three coating and one baking (3C1B) procedure, wherein viscosity of the intermediate coating composition is controlled, and furthermore, ratio of hydrophilicity to hydrophobicity of the resin in the intermediate coating composition is controlled, in order to significantly suppress sagging of the waterborne intermediate coating composition during the coating procedure. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10773276-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11634597-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10717895-B2 |
priorityDate | 2008-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |