Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_894efe14c7769edd97f630eaa1d7be3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ba47fcd2692501094afb7b6f13513f11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ddd82f56ea3c866b1936d08ae36a08c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_75249adb90a4cfa442d4751eea6ee07e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1f0a8aae261914e1d57965b3c9953544 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31938 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-067 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-577 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 |
filingDate |
2012-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2015-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0184f6834738ea4cce960a5d68bf2db1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b534718df42f7b865d8e79b7226d568e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_facf74c4853ff01ff9214525d2d6c53c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_904a13bb3075f6a3ae95f3c42df55a8d |
publicationDate |
2015-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-9138779-B2 |
titleOfInvention |
Multilayer coat and method for producing the same |
abstract |
Disclosed is a method for producing a multilayer coat characterized by including the steps of coating a substrate with an undercoating material to form an undercoat layer, coating the undercoat layer with an active energy ray-curing type ink in an ink-jet system, curing the active energy ray-curing type ink through active energy ray irradiation, and coating the cured active energy ray-curing type ink with a top coating material to form a top coat layer, wherein the surface free energy of the undercoat layer is γ s =20-50 mN/m, the active energy ray-curing type ink has a surface tension at 40° C. of 20-35 mN/m, and the top coating material has a surface tension at 25° C. of 20-50 mN/m, as well as a multilayer coat obtained by the production method. |