Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_203c4e4b9677c902919ad91d5fbb585e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c21c0488708f0c642cddcc6c1d5c3af3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bf353abc4ba8840f40d9c89db265131d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L81-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 |
filingDate |
2010-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-09-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c31d72c49b110a034cd9fd1c6bfbfe6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f3431c091e19873b72bf4e617dff897 |
publicationDate |
2014-09-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8841368-B2 |
titleOfInvention |
Nonflammable polyester resin composition and method for manufacturing such a resin composition |
abstract |
A method for manufacturing a nonflammable polyester resin composition comprising:n making a polymer mixture containing the following (A) to (E) components in a melted state pass through a space between two parallel faces, with a face-to-face distance x being set to 5 mm or less; (A) a polyester resin of 40 to 80% by weight; (B) a polycarbonate resin of 5 to 40% by weight; (C) a rubbery polymer of 5 to 30% by weight; (D) a polyphenylene sulfide resin and/or a phenol resin of 2 to 20% by weight; and (E) a phosphorus-containing acid ester compound and/or a polyamide resin of 0.1 to 25% by weight. |
priorityDate |
2009-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |