Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ee33b0e3e7398cf6fc957eeee59d510 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_60126a9321a5a22368138dc685a770b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_053d65570d03617ab306fbb9307e049a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9a47cfe61ab5cc1e9298c387ca9fe1a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a013f27aee93b16ee05c95b0d161b734 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-02 |
filingDate |
2009-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ca357bd588addd46b2be53f938ee080 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7698db66fe00a9f3d9a58e35eebbb946 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_216c771bcf679e2887b447586b07eb76 |
publicationDate |
2014-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8795550-B2 |
titleOfInvention |
Method for preparing cathode active material |
abstract |
A method for preparing a cathode active material includes mixing a phosphorus source material, a lithium source material, and a dispersing agent together to form a first liquid mixture. An iron powder is added into the first liquid mixture. The first liquid mixture with the iron powder therein is dried to achieve a precursor. The precursor is calcined in a protective gas at a temperature of about 600° C. to about 800° C. for more than about 2 hours. |