Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_83ce0f27bf1c28cf6b90abe63bdae352 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e4791215e86dbe5e8995e720fac881e2 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3016 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B42D25-328 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B42D25-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B42D25-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B42D25-364 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 |
filingDate |
2010-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7fe3ed492e75bc27da50c57d1478d27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8ea6b5ab22a35df059fffaffd7fa445 |
publicationDate |
2014-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8748068-B2 |
titleOfInvention |
Method of producing patterned birefringent product and birefringent pattern building material |
abstract |
A method of producing a patterned birefringent product, comprising at least steps [1] to [3] in this order:n [1] producing a birefringent pattern building material comprising at least one optically anisotropic layer, which is formed by a process including: coating and drying a composition containing at least one rod-like liquid crystalline compound having at least two reactive groups and at least one chiral agent to form a cholesteric liquid crystal phase; and then subjecting the cholesteric liquid crystal phase to heating or exposure to radiation to form the optically anisotropic layer containing a polymer fixed by polymerization and fixing; [2] subjecting the birefringent pattern building material to a patterned exposure to light; and, [3] baking a laminate obtained after the step [2] at 50° C. or higher and 400° C. or lower. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9664833-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9784894-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11745420-B1 |
priorityDate |
2009-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |