Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e919f12a278703c859a08ce75aaff9a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d3bec0f856686e2bca8ac85d3c834a92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f337d170664ce6289b38b0b0f92d2eac http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_21d2c2d5682f73843009e2f25ee33ea7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6d64bf8e335648080280b98f760c54e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b22450551e5992f40d922353288cd07f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c7a2bdb14993fe8c0f32016ee48716e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M12-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-244 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-364 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-4235 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M12-06 |
filingDate |
2010-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14a701f8de258f08a2073c06fd2a2782 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54b2481a55f35e4364c4dd80cb7f886b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_331d98a4d7c1e76c350459ab4a5eed0f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19151d13ea556bc87bc69374899376ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f27b598391e95984fb9278afb8d5d9aa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_989ae8f9fbb3f47082b69a35ba7c0e90 |
publicationDate |
2014-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8691439-B2 |
titleOfInvention |
Alkaline cell with performance enhancing additives |
abstract |
Alkaline electrochemical cells having extended service life and acceptable gassing and corrosion properties are disclosed. An amphoteric surfactant can be incorporated into the gelled anode mixture of an alkaline electrochemical cell, optionally with an organic phosphate ester surfactant or a sulfonic acid type organic surfactant or both. Zinc particles having a defined distribution of particle sizes can also be incorporated into a zinc anode. The electrolyte included, in the anode mixture can have a reduced hydroxide concentration. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10276869-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10158118-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10910647-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10547059-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11316159-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11081696-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11764357-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9793543-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9793542-B2 |
priorityDate |
2002-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |