Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbaf303c809f2f0c0a0d860d329fadbd |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1338 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31786 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D22-00 |
filingDate |
2012-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_db0bd1966029c16a2e0ab7300480ca10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_832df1a98c77fbeddb3cf5653724a15c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39e1aea9d71df20554c0034f2fdfc8a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15dca6192b25e34534492c9f921e2ab1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_633f1253f8f44a683d4a7b52f82e6ae0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9610f8a7da7d06da1aeec7702b18ad24 |
publicationDate |
2014-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8668970-B2 |
titleOfInvention |
Use of an antimony-free polyester film for producing film bags and film tubes with high heat resistance |
abstract |
Film bags or film tubes formed from biaxially oriented film including less than 10 ppm of antimony and having a haze of less than 10% are provided. The films have an ultimate tensile strength of more than 100 N/mm 2 ; have a difference in the ultimate tensile strength in MD and TD of less than 180 N/mm 2 ; have a tensile strain at break of more than 50%; a tensile strain at break of more than 260%; have a yellowness index b* of less than 2.5; have a lightness L*>85; include from 50 to 15 000 ppm of free-radical scavenger; have an SV of at least 600 after ovening; have a tensile strain at break of >5% after ovening; have a film thickness of from 6 to 26 μm; and include more than 90% by weight of polyester. |
priorityDate |
2011-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |