Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e443fcd44793752f156437bbfd4c8603 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14039171e1a63a17b423dc522eb2dec2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2982 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2998 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-14 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F120-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-12 |
filingDate |
2010-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5682a2df12b4f899e73df2b62b24bf74 |
publicationDate |
2013-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8617708-B2 |
titleOfInvention |
Methacrylic resin, molded article thereof, and method for producing methacrylic resin |
abstract |
A methacrylic resin, including 80 to 99.5% by mass of a methacrylic acid ester monomer unit, and 0.5 to 20% by mass of other vinyl monomer unit which is copolymerizable with at least one of the methacrylic acid ester, wherein the methacrylic resin satisfies the following conditions (I) to (III):n (I) having a weight average molecular weight measured by gel permeation chromatography (GPC) of 60,000 to 300,000; (II) having a content of a molecular weight component 1/5 or less the peak molecular weight (Mp) obtained from a GPC elution curve, said content being 7 to 40% based on a region area ratio obtained from the GPC elution curve; and (III) having an angle of repose of 20 to 40°. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9725588-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9481010-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2019241689-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11155662-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016264771-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10197724-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3885371-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11180593-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015111046-A1 |
priorityDate |
2009-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |