Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c3cd8354954fbb44ba8549683fc0207a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3b8b777d3f12429e26826f5746e81fa4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18920e888cdd4ea83da9e00cd7189f3d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9175beffe5ba5c5ad32e883b1ee612dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eacdb73fa0a1f80eddb8ed1b8cdcf06b http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2ab1bae0f7bde4aec820e97ad7c8aa2 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C8-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C8-30 |
filingDate |
2011-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45a980734dc7729b83eda3d53e7adc61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71c89c8527539ea691662c55850d664f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9cb913ef06b147039fe23f33278b284 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ced88c4278baa61c3c897cd59ce62b1e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae7a979d401744641732cb60bc139719 |
publicationDate |
2013-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8608868-B2 |
titleOfInvention |
Method for improving surface mechanical properties of non-austenitic stainless steels |
abstract |
A method for improving surface mechanical properties of non-austenitic stainless steels comprises steps of: providing a non-austenitic stainless steel material; placing the non-austenitic stainless steel material in an environment containing at least one austenite-stabilizing element, and implanting the austenite-stabilizing elements into a surface of the non-austenitic stainless steel material to form a modified layer enriched with the austenite-stabilizing elements; and placing the non-austenitic stainless steel material in a carbon-bearing atmosphere to make the modified layer in contact with the carbon-bearing atmosphere, and maintaining the non-austenitic stainless steel material at a carburizing temperature below 600° C. to implant carbon into the modified layer to form a carburized layer. The carburized layer enhances the surface hardness of the non-austenitic stainless steel material and enables it to apply to decorative components or structural components demanding high abrasion resistance, high surface hardness, and high corrosion resistance. |