Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2e2d0ef5791f2d4427893408d969c30d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a56cfb78165f255ba63fad4fdc06d19e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dcd8cece121b9a57306e03c721519fcd http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_005748c4743df899b303e5b5c39e9a66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_97b1e0ffe10a59f156668988f53ca674 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2333-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-128 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 |
filingDate |
2009-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc4b910c27abf34c3cc3846c87b61f21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd64a4b57c55511537544a1bcef036d2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b5e6a021b115da8105a6f4bccfa175e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_615a46e9915813c22471c6e2bfe5ab7d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b57ca4241b5bc5eed14610bc3c0fa6d |
publicationDate |
2013-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8546492-B2 |
titleOfInvention |
Surface treatment method for water-absorbing resin and production method for water-absorbing resin |
abstract |
The present invention provides a surface treatment method for a water-absorbing resin comprising three steps of: 1) a humidifying and mixing step for mixing a base polymer and a surface cross-linking agent solution to obtain a "humidified substance"; 2) a pretreatment step for raising temperature of said humidified substance to obtain a "pretreated substance"; and 3) a surface cross-linking reaction step for cross-linking said pretreated substance to obtain a surface cross-linked "water-absorbing resin"; wherein dew point in the pretreatment step of the above 2) is from 50° C. to 95° C., and temperature of said humidified substance is raised from temperature below the dew point up to a temperature of 10° C. higher than the dew point. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11459431-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014088012-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20150091363-A |
priorityDate |
2008-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |