abstract |
A block copolymer or graft copolymer with weight-average molar mass M w of at least 100 000 g/mol, comprisingn a) at least one block S composed of from 95 to 100% by weight of vinylaromatic monomers and from 0 to 5% by weight of dienes, and b) at least one copolymer block (S/B) A composed of from 63 to 80% by weight of vinylaromatic monomers and from 20 to 37% by weight of dienes, with glass transition temperature Tg A in the range from 5 to 30° C.,n nwhere the proportion by weight of the entirety of all of the blocks S is in the range from 50 to 70% by weight, based on the block copolymer or graft copolymer, and also mixtures thereof, and their use. |