abstract |
A method of using heat-resistant hollow sphere polymers having at least on crosslinked polymer stage, and having a core stage that has been swollen with a volatile base, in applications in which the hollow sphere polymer is exposed to temperatures of from 100° C. to 350° C., is provided. Articles made by the method are also provided. |