Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cea139ad438b9ce7d33159d45b154c6b http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e86ce5aa8f9f6fdb60f4b10a449a0ce5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_07c9542186133097bd6bbb7d92393090 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1920750069777383427d4b90094aca07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_668e54de57f9774a486775032f06d187 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_64ec186f64fe5e7206fabb1601cd7cc5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C11-0007 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C3-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C1-00 |
filingDate |
2006-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2012-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67ea81214473361cdd0062acc9a61e75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b15df96e2fd49281de051c7c4511152 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b59251659e9e9757ac9766c1b6e970f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2dd67c1bfcd5f021a3a955aa5bea83c2 |
publicationDate |
2012-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8092647-B2 |
titleOfInvention |
Method for treating lignocellulosic materials |
abstract |
The present invention is a method for producing a pulp from a fibrous lignocellulose material or source using a treatment or pretreatment step which exposes the material to oxalic acid derivatives, particularly dialkyl ester derivatives, particularly in the vapor phase. Once treated, the material may be refined using any one of the several pulping methods to produce a final pulp product and the production of the product is accompanied by strength increases in paper made from the pulp and energy savings in making the pulp, hi addition the treatment or pretreatment produces a soluble carbohydrate source and other components (e.g. acetic acid, other wood components) for further product development. In certain cases a pulp product is not produced and all of the carbohydrate present in the lignocellulose is converted into soluble sugars. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015136344-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9951363-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014052763-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9273431-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10006166-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9850512-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9115468-B2 |
priorityDate |
2005-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |