http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7923074-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b40c8ccc1611e7305ad1c8d397081ed7 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-34928 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 |
filingDate | 2010-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48593f2a5b65caa90498d7579d2a5358 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_849cc77610b02dd9f3dd9499a1493383 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a23281867318f3ccec412625b279a22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2bcb7361ab31dc98148af55b13a5f650 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83eaa48b5a785509fd99dafad721f7e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bbb85835b8fe6970dd8caea40947eb3 |
publicationDate | 2011-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7923074-B2 |
titleOfInvention | Method for preparing a vehicle interior material |
abstract | A method for preparing a vehicle interior material comprises the steps of feeding 100 parts by weight of phosphorus and nitrogen-containing non-halogen flame retardant particles and 0.1 to 20 parts by weight of hydrophobic inorganic oxide fine particles having hydrophobic groups and having an average particle size of 0.001 to 5 μm to a mixer equipped with a high-speed agitation means having a revolution capability of about 100 to 5,000 rpm, agitating and mixing the phosphorus and nitrogen-containing non-halogen flame retardant particles and the hydrophobic inorganic oxide fine particles to produce the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles, mixing 100 parts by weight as solids of a synthetic resin emulsion and 1 to 300 parts by weight of the phosphorus and nitrogen-containing non-halogen flame retardant particles coated with the hydrophobic inorganic oxide fine particles to produce a coating composition, coating the coating composition onto the vehicle interior material, and drying the coated vehicle interior material. |