http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7863364-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1f8713f6ace083308920724981592661 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-142 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 |
filingDate | 2006-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d94aa8c4072d2330cff193ab7bd2cb3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7637094d688f5fa95852c98968c89391 |
publicationDate | 2011-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7863364-B2 |
titleOfInvention | Process for making dynamically-loaded articles comprising propylene-based elastomers, composition for use in such processes, and article made using such processes |
abstract | The invention relates to a process for making an article subject to dynamic loading, the process comprises: (i) shaping a polymer-containing composition in the green state, the composition comprising (a) a continuous phase of a polymeric component of at least 15 wt %, based on the total weight of the polymer component of a propylene elastomer having a heat of fusion of less than 70 J/g and an isotactic triad tacticity of 50 to 99% and optionally containing units derived from a diene, the polymeric component having a density of less than 0.9 g/cm 3 and (b) from 20 to 120 phr, preferably 30 to 100 phr, most preferably 40 to 90 phr based on the total weight of the polymer component of a reinforcing filler component; and (c) a peroxide curative. The composition is combined with a fibrous reinforcement which is then cured to a cure state as determined by ODR @ 170° C., 30 min MH-ML of from 5 to 80 dNm. The invention especially relates to such processes when providing under Demattia testing conditions a crack length of less than 15 mm at room temperature over 90K cycles, preferably 10 mm, more preferably 7 mm, and most preferably 4 mm, and a 10% modulus of 0.7 to 10 MPa, preferably 1.4 to 9 MPa and most preferably 2 to 8 MPa. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10760646-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015211600-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8178031-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8431065-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011077317-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9487653-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018223953-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8703030-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8765832-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9328798-B2 |
priorityDate | 2006-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 151.