Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8268e39ce70ff2ad19742e2a21d5a90c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-494 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-488 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2505-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-2623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-2861 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06N3-0009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04B21-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06N3-0029 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04B21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04B23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A63B71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F41C27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-04 |
filingDate |
2005-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2010-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e1a57af747facd3882555f6328389cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bed55c7e7e855c4db8ce0f257f27e131 |
publicationDate |
2010-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-7851388-B2 |
titleOfInvention |
Lead pellet recovery fabrics |
abstract |
The invention provides methods for finishing knitted fabrics and fabrics finished by the novel process. In one embodiment, the method of finishing a knitted fabric includes the steps of: (a) stretching the fabric above about 5% but less than about 25% in width, and above about (−)7% but less than about 10% in length, (b) heat-setting the fabric to the stretched width and length at a temperature above about 120 degrees Centigrade and lower than about 250 degrees Centigrade, and (c) applying a polymeric protective binder coating resin to the fabric at a concentration of at least 5% but less than 25% based on the weight of the fabric. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10012483-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10012482-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2022259777-A1 |
priorityDate |
2005-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |