Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F110-04 |
filingDate |
2005-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2010-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a45cc5c8023821556f7435a8310069f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59038a3c2c81a888442ac5fef0921469 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6416ddba04df41e8dbdc25899e7a86c8 |
publicationDate |
2010-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-7795353-B2 |
titleOfInvention |
Method for producing a modified propylene polymer |
abstract |
Disclosed is a method for producing a modified propylene polymer, the method comprising heating a mixture of 100 parts by weight of a propylene polymer (A) defined below and from 0.1 to 50 parts by weight of an ethylenically unsaturated bond-containing monomer (B) in the presence of from 0.01 to 20 parts by weight of an organic peroxide (C); propylene polymer (A) being a propylene polymer composed of from 0.5 to 90% by weight of a propylene polymer component (A1) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of from 5 dl/g to 15 dl/g and from 10 to 99.5% by weight of a propylene polymer component (A2) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of not less than 0.1 dl/g but less than 5 dl/g. |