http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7776778-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3b1bfade89092e93f2eee59b87ffe1c5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_baa1c603bcb1420d238da46616bcefd6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ebf208e8ed2334f3044b3df8c26d5982 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1019 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C5-3332 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10G25-00 |
filingDate | 2005-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2010-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b66474f2c1c8d9e1bdb3f679eb8d29cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1d30678580debfd95b3137b7d98de64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4aff00180dd0e8ca1f7b02be65a5b9fc |
publicationDate | 2010-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7776778-B2 |
titleOfInvention | Hydrocarbon conversion catalyst and methods for making and using it |
abstract | X-ray amorphous carbon is formed by evaporating carbonic material. The evaporation of carbonic material is conducted in a helium atmosphere at a supply energy flow in the range of 50 to 300 W/mm 2 . The energy is generated, for example, by means of an electric arc. The X-ray amorphous carbon has a starting temperature of an air oxidation, T so , ≦320° C.; a temperature of maximal rate of an air oxidation, T omr , ≦590° C.; a temperature of end of an air oxidation, T eo , ≦630° C.; an initial rate of non-catalytic hydrogenolysis by molecular hydrogen at 700° C., V hin , ≧2.08% mass of carbon/h. Upon contact in a solution, 1 g of X-ray amorphous carbon consumes an amount equal to or greater than 16 mmole of MnO 4 − ions. Catalysts based on the X-ray amorphous carbon are used in hydrocarbon dehydrogenation and dehydrocyclization reactions. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2712446-C1 |
priorityDate | 2003-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.