http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7572404-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_574bc8fd24e08fc5a292d012c5a28e48 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2120-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6685 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 |
filingDate | 2006-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_341ace7699bab8690f53d1cad6dadab3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47d56b55b84eec3f2495e698c0496896 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed3a26d116b3106572288d9399b11b13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f69701bf1240e3f45e60e71440efb307 |
publicationDate | 2009-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7572404-B2 |
titleOfInvention | Vehicle interior article of skin-integrated laminate, method for manufacturing non-foaming polyurethane resin and method for manufacturing skin-integrated laminate using the same |
abstract | The present invention is directed to skin-integrated laminates and their use as vehicle interior articles, in which the laminates feel comfortable to the touch and have a high quality of external appearances. The invention also relates to a method for manufacturing these non-foaming polyurethane resins for use as design skins in vehicle interior articles and to a method for manufacturing a skin-integrated laminate from these non-foaming polyurethane resins, with both methods having increased productivity and lower cost, and without any adverse influence on the work environment. The non-foaming polyurethane resin forms a design skin surface by a reaction injection molding process, in which (I) a polyol mixture of (1) a polyol, (2) a chain extender which is 1-methyl-3,5-diethyl-2,4-diaminobenzene and/or 1-methyl-3,5-diethyl-2,6-diaminobenzene, (3) a catalyst, and (4) optionally, an auxiliary agent, and (II) a polyisocyanate compound, are reacted. The surface hardness of the non-foaming polyurethane resin, as measured by an Asker A hardness meter, is from 30 to 70. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009075084-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009267254-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8057727-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8071208-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8316520-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011119882-A1 |
priorityDate | 2005-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 117.