http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7537805-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41C1-1016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41C2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41C2210-24 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41C1-1008 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41F23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41F1-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 |
filingDate | 2006-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00133eb4cdb28bd579268b51db16d71f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4da9d9458261c076a3457e7b057eba6d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9949f5cb07a5d8d41ffb500ebbdda1c5 |
publicationDate | 2009-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7537805-B2 |
titleOfInvention | Method for producing coated article |
abstract | In the present invention, a coating liquid satisfies the liquid physical property conditions: (A) in the drying process, after the solid content concentration in the coating liquid is increased to 15% by mass or more by drying the coating film, or after the start of drying when the solid content concentration in the coating liquid is 15% by mass or more at the time of coating; (B) the shear viscosity of the coating liquid becomes 5 mPas or more for the shear rate of 10 3 sec −1 or less; (C) the value obtained through dividing by the average viscosity the first differential coefficient, the increase coefficient of the increase rate of the shear viscosity relative to the increase rate of the solid content concentration is 0.15 or more; and (D) the second differential coefficient, an additional increase coefficient of the increase coefficient relative to the solid content concentration is positive. |
priorityDate | 2005-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links