http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7410745-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-03594 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-0056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-03552 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-03558 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-0051 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C5-17 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49845 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49818 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-16 |
filingDate | 2003-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a93e11bb37ccc4282f901ec7f356213 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2af0593575e2be283efa26e95abb9a8d |
publicationDate | 2008-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7410745-B2 |
titleOfInvention | Photothermographic material and image forming method using same |
abstract | The invention provides a photothermographic material including: a support and an image-forming layer including a non-photosensitive silver salt, a photosensitive silver halide, a binder, and a reduction agent disposed on the support, wherein a silver iodide content in the photosensitive silver halide is in a range from 40 mol % to 100 mol %; and an average sphere-equivalent diameter of the photosensitive silver halide is in a range from 0.3 μm to 5.0 μm. The photothermographic material may further include a silver iodide complex forming agent as a compound which substantially reduces visible light absorption caused by the photosensitive silver halide after thermal development. At least 50%, in terms of a projected area, of the photosensitive silver halide may be occupied by tabular silver halide grains having an aspect ratio of from 2 to 50 and being deposited with a silver salt in an epitaxial growth manner. |
priorityDate | 2002-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 1777.