http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7384468-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_34fbeb1e614ea098731393cc639cd372 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D195-00 |
filingDate | 2004-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99a73ccefce2e4f6e6048292966d4290 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3abee50b1709446db018d382dc61f5e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee1d26078735a26d0b9dbd72852ed56d |
publicationDate | 2008-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7384468-B2 |
titleOfInvention | Asphalt/aggregate composition of enhanced adhesion |
abstract | An asphalt/aggregate composition having enhanced adhesion characteristics and its preparation. An asphalt base material is heated to a molten state in order to permit mixing of the asphalt with added components. A heavy metal soap is incorporated into the asphalt base material to enhance the adhesion of the asphalt base material with an aggregate component which is mixed with the asphalt base material to provide an asphalt/aggregate blend. The asphalt and aggregate can be blended together in a mixing chamber to provide a fluid asphalt/aggregate concrete which is then dispensed on a substrate surface or the asphalt base material and aggregate components can be separately applied to the substrate surface to provide the ultimate asphalt/aggregate concrete. The heavy metal soap is a C 14 -C 18 heavy metal soap such as zinc stearate. Zinc oxide may also be added to the asphalt base material in an amount which is less than the amount of zinc stearate. The asphalt base material may be polymer-modified asphalt and may incorporate a crumb rubber component to provide a rubber-modified asphalt. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10655015-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011269877-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9018279-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9458320-B2 |
priorityDate | 2004-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.