Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2baf849d216e689ecc40ccc931a7a7bc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-17 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-0266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-128 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-14 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-30 |
filingDate |
2004-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2008-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_471977c60b11508bfea82d5b5d101552 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02f2e04392c938516b26a11c6cee4053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_939947f32ed0893c445bf80e694d36e0 |
publicationDate |
2008-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-7341678-B2 |
titleOfInvention |
Charge-transporting varnish |
abstract |
A charge-transporting varnish is disclosed which comprises a charge-transporting material composed of an oligoaniline compound represented by the formula (1) below and at least one kind of solvent. In this charge-transporting varnish, the charge-transporting material is dissolved or homogeneously dispersed in the solvent. By using this varnish, a charge-transporting thin film having excellent conductive characteristics can be formed through a short-time firing. In particular, when the varnish is applied to an OLED element or a PLED element, the resulting element can achieve excellent element characteristics such as low driving voltage, high luminous efficiency and long life |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9172048-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7455792-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9251923-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005082514-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007205400-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006115652-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11563176-B2 |
priorityDate |
2003-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |