http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7074293-B2

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e9dbff9afcea85c0a3d68f16fd74c004
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2037-243
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2551-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-164
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-26
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C65-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B31F5-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-08
filingDate 2004-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2006-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f04728a130e59deba57950348bbcd59
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_419405a28bd85a2512f6523be3d7b5df
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b86fdd953a8caed358991c4b1544fda
publicationDate 2006-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-7074293-B2
titleOfInvention Method to improve film property
abstract A method improves the property of films including a release film and a protective film. After separating from the release film, the protective film is bonded with a TAC (Triacetyl Cellulose) film and then processed by coating, such as with an anti-reflecting coating, an anti-glaring coating and a surface hardening treatment, and by drying in an oven. The protective film is separated from the TAC film. The waste of material, which resulted from cracks, snaps and bends of the film, is avoided in the process. Furthermore, practice costs are low, and additional expensive apparatus or treatment are not necessary for a simplified procedure of the method.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009054874-A1
priorityDate 2004-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004169290-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-3904797-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6261665-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-498318-B
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6767630-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2003064579-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2003198807-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-546728-B
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5000809-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID410507379
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226411475
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226411474
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID19046907
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID18755810
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15066111
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID44263853
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226411476

Total number of triples: 50.