Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6b822ee046eb6c45d1e3bd9ce9c1782e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-311 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-611 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K2102-3026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-324 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K85-631 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-171 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-26 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-26 |
filingDate |
2003-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2005-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ff5f9fe95e568ddab1aae99cebe6ef2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b2793f5b5e5d5167cccd5f69b6cd4732 |
publicationDate |
2005-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6838836-B2 |
titleOfInvention |
Light emitting device and manufacturing method therefor |
abstract |
To provide a light emitting element having a top emission structure, which can be easily manufactured without considering an ionization potential of an electrode (particularly an electrode in contact with a substrate) and a manufacturing method therefor. A light emitting device having the top emission structure according to the present invention includes: a first electrode ( 101 ) formed of general-purpose metal (specifically, a wiring material such as Ti or Al) having a light-shielding property or reflectivity; a conductive polymer layer ( 102 ) formed by applying a conductive polymer material onto the first electrode ( 101 ); an electroluminescence film ( 103 ) formed in contact with the conductive polymer layer ( 102 ); and a light-transmissive second electrode ( 104 ) formed on the electroluminescence film 103 , in which the conductive polymer layer ( 102 ) is formed of materials including a redox polymer etc., while being free of problems regarding work function (as shown in FIG. 1 A). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014118653-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005104510-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7108574-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006234416-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7537878-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2003062826-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005136784-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009315026-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7407422-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010267208-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8729832-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013271036-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9613568-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009121341-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7126267-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005236969-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2005264174-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7075228-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7193359-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006040200-A1 |
priorityDate |
2002-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |