abstract |
Process for preparing a polyurethane material having no glass transition temperature below 25 C, which process involves using a polyoxyethylene polyoxypropylene polyol having a high oxyethylene content and a polyisocyanate having a high 4,4′-diphenylmethane diisocyanate (4,4′-MDI) content, wherein the reaction is conducted at an isocyanate index of 80 to 140. |