Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_114e4423ec77cbc8dab9d0a98909704e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-01838 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B37-018 |
filingDate |
2001-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2004-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3cadb8ce738b9e9600bf9847814a654 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f163eec8b83b00aa2737e4b7b35820d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e619b049a46584b9f2743c25f8837a2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9312dd3e6d7a80b03f8b3e0ed432dae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c498002c6572977173158e7f1ebabb76 |
publicationDate |
2004-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-6751990-B2 |
titleOfInvention |
Process for making rare earth doped optical fiber |
abstract |
The present invention provides an improved process for making rare earth doped preforms and fibers by a combination of MCVD technique and solution doping method, said method comprising developing matched or depressed clad structure inside a silica glass substrate tube followed by deposition of unsintered particulate layer containing GeO 2 and P 2 O 5 for formation of the core and solution doping by soaking the porous soot layer into an alcoholic/aqueous solution of RE-salts containing co-dopants like AlCl 3 /Al(NO 3 ) 3 in definite proportion, controlling the porosity of the soot, dipping period, strength of the solution and the proportion of the codopants to achieve the desired RE ion concentration in the core and minimize the core clad boundary defects and followed by drying, oxidation, dehydration and sintering of the RE containing porous deposit and collapsing at a high temperature to produce the preform and overcladding with silica tubes of suitable dimensions and fiber drawing to produce fibers. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106006599-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10040714-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11407671-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106006599-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010109494-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014178063-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012201504-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009269605-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6851281-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2003182970-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8649650-B2 |
priorityDate |
2001-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |