http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6649100-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e643df164d408263905077a4d3016558 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2973 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-0018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-731 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-52 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C69-001 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C69-00 |
filingDate | 2000-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2003-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09c14514bb561d5d9f66531b79495f49 |
publicationDate | 2003-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-6649100-B2 |
titleOfInvention | Method of producing rubber thread for golf ball and rubber thread for golf ball |
abstract | A method of producing a rubber thread for a golf ball includes (a) an extruding process of extruding a rubber composition in the shape of a sheet by using an extruder (2) to obtain a sheet material (6); (b) a rolling process of rolling the sheet material (6) to make it thin to obtain a thin sheet material (10); (c) a cross-linking process of cross-linking the thin sheet material (10) to obtain a cross-linked sheet material; and (d) a cutting process of cutting the cross-linked sheet material to obtain a rubber thread. The rolling process is performed successively to the extruding process. The thickness t1 of the sheet material (6) obtained in the extruding process is set to a range of 1 mm to 8 mm both inclusive. The thickness t2 of the thin sheet material (10) obtained in the rolling process is set to a range of 0.3 mm to 0.6 mm both inclusive. |